Polymer Property : Thermal Conductivity = 8.3816 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.2097 W/m-K

@Temperature 800 °C
8.3816 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Chosun Refractories HACT-180 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).