Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.2097 W/m-K @Temperature 800 °C |
8.3816 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories HACT-180 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |