Thermal Properties Metric English Comments
Thermal Conductivity 9.08 W/m-K

@Temperature -73.0 °C
63.0 BTU-in/hr-ft²-°F

@Temperature -99.4 °F
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy
MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers..