Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 9.08 W/m-K @Temperature -73.0 °C |
63.0 BTU-in/hr-ft²-°F @Temperature -99.4 °F |
|
H.C. Starck MP35N® Nickel/Cobalt/Chromium/Molybdenum Alloy MP35N is a nickel-cobalt based alloy of the Multiphase® alloy system that has ultra high strength, toughness, ductility, biocompatibility, and outstanding corrosion resistance. H.C. Starck offers.. |