Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.930 - 1.13 W/m-K @Temperature 600 °C |
6.45 - 7.84 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 85 PD REPAIR Moldable Refractory Material Description: Curas 85 PD Repair is a phosphate bonded moldable based on sintered bauxite. It has been specially developed for aluminum melting and holding furnaces. However, it can be applied on any.. |
|||
Thermal Conductivity | 0.930 - 1.03 W/m-K @Temperature 1400 °C |
6.45 - 7.15 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast CURON 160 Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and maintains its strength up to high temperatures. In addition Curon 160 has an excellent thermal sh.. |
|||
Thermal Conductivity | 0.930 - 1.13 W/m-K @Temperature 600 °C |
6.45 - 7.84 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS 90 SPF Moldable Refractory Material Description: Curas 90 S PF is a moldable which is characterized by its outstanding abrasion resistance (acc. to ASTM C-704: < 3 cc). This material is supplied as a powder which only has to be mixed .. |
|||
Thermal Conductivity | 0.930 W/m-K @Temperature 800 °C, Time 10800 sec |
6.45 BTU-in/hr-ft²-°F @Temperature 1470 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST C SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 0.930 W/m-K @Temperature 400 °C, Time 10800 sec |
6.45 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST K High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 0.930 W/m-K @Temperature 400 °C, Time 10800 sec |
6.45 BTU-in/hr-ft²-°F @Temperature 752 °F, Time 3.00 hour |
|
Sharadaa Ceramics REFCAST K SUPER High Alumina Castables Description: We bring to our clients a qualitative range of Dense Alumina Castables that are conventional castable of medium purity. These castables cater to the application needs of various industr.. |
|||
Thermal Conductivity | 0.930 W/m-K @Temperature 1671 °C |
6.45 BTU-in/hr-ft²-°F @Temperature 3040 °F |
|
Zircar Ceramics ZIRALCAST 95 Alumina Refractory Castable Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applica.. |
|||
Thermal Conductivity | 0.930 W/m-K @Temperature 790 °C |
6.45 BTU-in/hr-ft²-°F @Temperature 1450 °F |
|
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |