Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 6.50 - 8.50 W/m-K @Temperature 600 °C |
45.1 - 59.0 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |