Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 8.00 - 10.0 W/m-K @Temperature 100 °C |
55.5 - 69.4 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast FLUCON 160 K Dense Self Flowing Refractory Castable Description: Flucon 160 K is a self-flowing low cement castable based on silicon carbide. This castable is characterized by high strength high abrasion resistance and excellent thermal shock resista.. |
|||
Thermal Conductivity | 8.00 W/m-K @Temperature 400 °C |
55.5 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
CoorsTek ADOS-90R 91% Alumina Thick Film Substrate This 91-percent alumina (nominal) formulation offers a dark brown body for special applications. Applications: thick films and lasers |