Thermal Properties Metric English Comments
Thermal Conductivity 0.84910 W/m-K

@Temperature 540 °C
5.8832 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).