Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.77931 W/m-K @Temperature 800 °C |
5.3997 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Chosun Refractories CT-140S Fireclay Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.77931 W/m-K @Temperature 260 °C |
5.3997 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Chosun Refractories HACT-160 High Alumina Castables Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |