Polymer Property : Thermal Conductivity = 0.77931 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.77931 W/m-K

@Temperature 800 °C
5.3997 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.77931 W/m-K

@Temperature 260 °C
5.3997 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).