Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 36.8 W/m-K @Temperature 399 °C |
255 BTU-in/hr-ft²-°F @Temperature 750 °F |
hardness of 40 HRC |
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening.. |