Thermal Conductivity 36.8 W/m-K

@Temperature 399 °C
255 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardness of 40 HRC
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel ALVAR 14 is characterized by: Good toughnessGood resistance to high thermal stresses Good stability in hardeningGood through-hardening..