Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 31.2 W/m-K @Temperature 300 °C |
217 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |