Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 31.2 W/m-K @Temperature 300 °C |
217 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Thermal Conductivity | 31.3 W/m-K @Temperature 21.1 °C |
217 BTU-in/hr-ft²-°F @Temperature 70.0 °F |
|
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |