Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.430 - 0.530 W/m-K @Temperature 1000 °C |
2.98 - 3.68 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar.. |