Thermal Conductivity 0.430 - 0.530 W/m-K

@Temperature 1000 °C
2.98 - 3.68 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar..