Polymer Property : Thermal Conductivity = 28.4 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 28.4 W/m-K

@Temperature 500 °C
197 BTU-in/hr-ft²-°F

@Temperature 932 °F
International Mold Steel Daido DRM1 Matrix High-Speed Steel
This tough matrix type high speed tool steel features high hardness and high tough Matrix type high speed tool steel vastly surpasses hot work die steels. DRM1 improves hot and warm die life by its ..
Thermal Conductivity 28.4 W/m-K

@Temperature 400 °C
197 BTU-in/hr-ft²-°F

@Temperature 752 °F
International Mold Steel DH31-EX Die Cast & Forging Steel
DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b..
Thermal Conductivity 28.4 W/m-K

@Temperature 900 °C
197 BTU-in/hr-ft²-°F

@Temperature 1650 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Thermal Conductivity 28.4 W/m-K

@Temperature 100 °C
197 BTU-in/hr-ft²-°F

@Temperature 212 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..