Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.3 W/m-K @Temperature 23.0 °C |
183 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 150 °C, Time 3600 sec |
183 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
+200°C/1 hr |
Epoxy Technology EPO-TEK® EK1000 Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 150 °C, Time 3600 sec |
183 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
+200°C/1 hr |
Epoxy Technology EPO-TEK® EK1000-MP Epoxy Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding .. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 150 °C, Time 3600 sec |
183 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
+200°C/1 hr |
Epoxy Technology EPO-TEK® EK2000 Epoxy Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance .. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 500 °C |
183 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER K294 MICROCLEAN AISI A11 Powder Metal Tool Steel Properties: Powder-metallurgical produced cold work tool steel with extremely high wear resistance, good toughness and high compressive strength. The latest generation of powder metal technology ena.. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 500 °C |
183 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 430 Ferritic Stainless steel AK Steel 430 combines good corrosion resistance and heat and oxidation resistance up to 1500°F with good mechanical properties. Typical consumer applications include automotive trim and molding, f.. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 500 °C |
183 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
Thermal Conductivity | 26.3 W/m-K @Temperature 500 °C |
183 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
AK Steel 434 Ferritic Stainless steel AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy's corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidati.. |