Polymer Property : Thermal Conductivity = 25.96 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 25.96 W/m-K

@Temperature 20.0 - 500 °C
180.2 BTU-in/hr-ft²-°F

@Temperature 68.0 - 932 °F
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..