Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 24.90 W/m-K @Temperature 93.3 °C |
172.8 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel 410 Chromium Steel Crucible 410 is a hardenable chromium steel which is adaptable for general purpose corrosion resisting and heat resisting applications. This grade is magnetic at times. Information provided by Cruci.. |
|||
Thermal Conductivity | 24.90 W/m-K @Temperature 93.3 °C |
172.8 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |