Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 23.0 W/m-K @Temperature 150 °C, Time 3600 sec |
160 BTU-in/hr-ft²-°F @Temperature 302 °F, Time 1.00 hour |
+ 200°C/1Hr |
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H14 4/4 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H15 Spring, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 0 Annealed, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Drawn Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature <=200 °C |
160 BTU-in/hr-ft²-°F @Temperature <=392 °F |
|
CLAL-MSX ARCAP Anticorrosion AP4 H12 1/2 hard, Rolled Copper Alloy Description: The AP4 grade is less easy to turn than the other grades of ARCAP. It can however be machined without more difficulty than the nickel chromium molybdenum steels.High Corrosion Resistanc.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 400 °C |
160 BTU-in/hr-ft²-°F @Temperature 752 °F |
hardened to 58 HRC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 400 °C |
160 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Assab Steels ASSAB XW-42 Cold Work Steel XW-42 is a high-carbon, high chromium tool steel alloyed with molybdenum and vanadium characterized by:High wear resistanceHigh compressive strength High hardness after hardeningGood through-hardeni.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 10% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Thermal Conductivity | 23.0 W/m-K @Temperature 500 °C |
160 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |