Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.6 W/m-K @Temperature 200 °C |
226 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Thermal Conductivity | 32.6 W/m-K @Temperature 400 °C |
226 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER W400 VMR® H11 Hot Work Tool Steel W400 VMR is a low silicon, chromium-vanadium hot work tool steel which has been vacuum remelted to obtain the highest uniformity, the best cleanliness of tool steel. The material is characterized:E.. |
|||
Thermal Conductivity | 32.6 W/m-K @Temperature 400 °C |
226 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 468°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |
|||
Thermal Conductivity | 32.5 W/m-K @Temperature 400 °C |
226 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |
|||
Thermal Conductivity | 32.6 W/m-K @Temperature 300 °C |
226 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |
|||
Thermal Conductivity | 32.6 W/m-K @Temperature 400 °C |
226 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Carpenter AerMet®-for-Tooling Tool Steel, Double Aged 482°C Data provided by Carpenter Technology Corporation.This is a double vacuum melted alloy with high hardness and strength combined with exceptional ductility and toughness. The alloy is designed for c.. |