Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 31.8 W/m-K @Temperature 343 °C |
221 BTU-in/hr-ft²-°F @Temperature 650 °F |
|
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
Thermal Conductivity | 31.9 W/m-K @Temperature 500 °C |
221 BTU-in/hr-ft²-°F @Temperature 932 °F |
|
Bohler-Uddeholm BÖHLER W360 ISOBLOC® Hot Work Tool Steel BÖHLER W360 ISOBLOC was developed as a tool steel for dies and punches in warm and hot forging. The steel can be used for a variety of applications where hardness and toughness are required. Prope.. |
|||
Thermal Conductivity | 31.8 W/m-K @Temperature 302 °C |
221 BTU-in/hr-ft²-°F @Temperature 575 °F |
|
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |