Polymer Property : Thermal Conductivity = 20.23 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 20.23 W/m-K

@Temperature 93.3 °C
140.4 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..
Thermal Conductivity 20.23 W/m-K

@Temperature 93.3 °C
140.4 BTU-in/hr-ft²-°F

@Temperature 200 °F
Crucible Steel 431 Chromium Steel
Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten..