Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 20.23 W/m-K @Temperature 93.3 °C |
140.4 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Thermal Conductivity | 20.23 W/m-K @Temperature 93.3 °C |
140.4 BTU-in/hr-ft²-°F @Temperature 200 °F |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |