Polymer Property : Thermal Conductivity = 2.97 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.97 W/m-K

@Temperature 25.0 °C
20.6 BTU-in/hr-ft²-°F

@Temperature 77.0 °F
COI Ceramics Nicalon™ CG SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..