Thermal Properties Metric English Comments
Thermal Conductivity 0.420 W/m-K

@Temperature 150 °C
2.91 BTU-in/hr-ft²-°F

@Temperature 302 °F
Pyrotek NAD-11 Structural Insulation Board
NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation ..
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 600 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 600 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 125 GM Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast...
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 600 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 1000 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 130 GM Refractory Insulating Castable
Description: Golite 130 GM is a standard, medium weight gunning castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast p..
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 1000 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 130 Refractory Insulating Castable
Description: Golite 130 is a standard, medium weight castable, combining a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast products. Al..
Thermal Conductivity 0.420 W/m-K

@Temperature 538 °C
2.91 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials BNZ-3000 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.420 W/m-K

@Temperature 1093 °C
2.91 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials PA 26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.420 W/m-K

@Thickness 3.17 mm,
Temperature 47.0 °C
2.91 BTU-in/hr-ft²-°F

@Thickness 0.125 in,
Temperature 117 °F
ASTM C518
3M E-FIS Fire Barrier Expantrol Flexible Intumescent Strip
3M Fire Barrier E-FIS has been designed to seal the air space between doors and frames and for glazing fire resistant glass to help prevent the passage of smoke and flames in the event of a fire. Wh..
Thermal Conductivity 0.420 - 0.520 W/m-K

@Temperature 100 °C
2.91 - 3.61 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 160 GM Refractory Insulating Castable
Description: Golite 180 GM is a gunning mix that can be used up to very high temperatures in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.