Thermal Properties Metric English Comments
Thermal Conductivity 0.395 W/m-K

@Temperature 1400 °C
2.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia Buster Blanket Alumina Blanket Insulation
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga..
Thermal Conductivity 0.395 W/m-K

@Temperature 1400 °C
2.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia Buster Blanket Alumina Blanket Insulation
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga..