Material Notes:
Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an organic fiber reinforcement. Both forms have useful properties up to 1600°C. These polycrystalline fiber blankets offer higher temperature capability, less shrinkage and greater chemical resistance than standard alumina-silica blankets. Buster Blanket is made by needling the Buster Mat with an organic fiber reinforcement. This additional processing results in a much denser, stronger and more durable flexible insulation. It is offered in both 1/2” and 1” standard thicknesses. Flexible Buster products are useful as insulation packing in furnace spaces, around furnace sight tubes & ports and as filler in expansion joints and masonry cracks.Features: Available in Two Different FormsLow Thermal ConductivityHighly RefractoryNon-RCF FibersLow Shrinkage up to 1500°C97% Pure AluminaAvailable “Off the Shelf”Information provided by Zircar Zirconia.
Physical Properties Metric English Comments
Bulk Density 0.0960 g/cc
0.00347 lb/in³
Thermal Properties Metric English Comments
Thermal Conductivity 0.315 W/m-K

@Temperature 1200 °C
2.19 BTU-in/hr-ft²-°F

@Temperature 2190 °F
0.395 W/m-K

@Temperature 1400 °C
2.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
0.476 W/m-K

@Temperature 1600 °C
3.30 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Melting Point 2038 °C
3700 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage <= 4.00 %

@Temperature 1500 °C,
Time 21600 sec
<= 4.00 %

@Temperature 2730 °F,
Time 6.00 hour
Component Elements Properties Metric English Comments
Al2O3 97 %
97 %
SiO2 3.0 %
3.0 %
Descriptive Properties Value Comments
Trace Impurities <0.5%
Trace Inorganics <3%