Polymer Property : Thermal Conductivity = 2.70 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 2.70 W/m-K

@Temperature 1100 °C
18.7 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 94 M Dense Refractory Brick
Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â..
Thermal Conductivity 2.70 W/m-K

@Temperature 100 °C
18.7 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast LP 80 A Dense Refractory Brick
Description: LP 80 is a low porosity brick based on sintered bauxite with an extremely high abrasion resistance and therefore very well suited for application in rotary cement furnaces.Remarks: This..