Thermal Conductivity 2.25 W/m-K

@Temperature 100 °C
15.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 70 K Dense Refractory Brick
Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values..
Thermal Conductivity 2.25 W/m-K

@Temperature 100 °C
15.6 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AK 70 A Dense Refractory Brick
Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s..