Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.25 W/m-K @Temperature 100 °C |
15.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Thermal Conductivity | 2.25 W/m-K @Temperature 100 °C |
15.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |