Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.10 W/m-K @Temperature 650 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 650 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 650 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 80 B Dense Refractory Brick Description: A brick made from very pure Guyana bauxite. For applications under severe working conditions such as electric arc furnace roofs.Remarks: This data represents average values, obtained fr.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 80 FM Dense Refractory Brick Description: This fused mullite based brick has a very good thermal shock resistance and an excellent resistance against liquid slags at high temperature.Remarks: This data represents average values.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 650 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 K Dense Refractory Brick Description: Corundum based bricks with a mullite bond. Application: rotating incinerator furnacesRemarks: This data represents average values, obtained from samples that were cut from standard bric.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 P1 Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. In order to optimized the resistance against aluminum attack the sum of Al2O.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 KP Dense Refractory Brick Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 85 PW Dense Refractory Brick Description: A phosphate bonded bauxite brick with outstanding erosion resistance and resistance against liquid aluminum. Application: aluminum holding furnaces.Remarks: This data represents average.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1100 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1000 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Warp direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1000 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Fill direction |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |
|||
Thermal Conductivity | 2.10 W/m-K @Temperature 1200 °C |
14.6 BTU-in/hr-ft²-°F @Temperature 2190 °F |
Thru-thickness |
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |