Thermal Properties Metric English Comments
Thermal Conductivity 2.80 W/m-K

@Temperature 100 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast AC 85-5 Dense Refractory Brick
Description: Excellent resistance against alkali- and metal slags. A good volume stability at very high temperatures. Application: chemical incinerators, combustion chambers for very high temperatur..
Thermal Conductivity 2.80 W/m-K

@Temperature 650 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AC 90-5 D Dense Refractory Brick
Description: A special quality with an extra ordinary resistance to alkali and metallurgical slags, a good resistance to thermal cycling, a good volume stability and high strength at high process te..
Thermal Conductivity 2.80 W/m-K

@Temperature 650 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast ACZ 85-5 D Dense Refractory Brick
Description: Special low porosity quality with excellent resistance against alkali- and metal slags, a good volume stability and a high strength and elasticity at very high temperatures. Application..
Thermal Conductivity 2.80 W/m-K

@Temperature 650 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 94 M Dense Refractory Brick
Description: This mullite bonded, corundum brick combines a very good thermal shock resistance with a low creep as well as with resistance against a large variety of slags. (after 50 hours at 1650Â..
Thermal Conductivity 2.80 W/m-K

@Temperature 100 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast LP 85 AM Dense Refractory Brick
Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad..
Thermal Conductivity 2.80 W/m-K

@Temperature 100 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast LP 85 M Dense Refractory Brick
Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs...
Thermal Conductivity 2.80 W/m-K

@Temperature 100 °C
19.4 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast LP 85 KP Dense Refractory Brick
Description: This mullite and phosphate bonded corundum brick has a very low porosity, a high strength and a good thermal shock resistance. This quality has a very good resistance against slag. Appl..