Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 25.6 W/m-K @Temperature 204 °C |
178 BTU-in/hr-ft²-°F @Temperature 399 °F |
|
Latrobe LSSâ„¢ H12 Hot Work Tool Steel (ASTM H12) TLS H12 hot work tool steel is a 5% chromium, general-purpose hot work steel that is characterized by excellent impact toughness. It contains less vanadium than the widely-used H13 hot work tool ste.. |
|||
Thermal Conductivity | 25.6 W/m-K @Temperature 1000 °C |
178 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Haynes 625SQ® Nickel Alloy Sheet Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â.. |
|||
Thermal Conductivity | 25.6 W/m-K @Temperature 540 °C |
178 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel Airdi 150 (AISI D2) is an air-hardening, high carbon, high chromium tool steel, heat treatable to HRC 60-62. It offers excellent abrasion resistance, due to a large volume of carbides in the microst.. |