Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
H900
Crucible Steel 15-5 Precipitation Hardening Stainless Steel
Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
H900
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
H900
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel
Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. ..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900
AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, ..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Annealed
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1075 (Heated 579°C)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150 (Heated 621°C)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1150M (Heated 760°C/2hr/AC then 621°C/4hr/AC)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base..
Thermal Conductivity 22.6 W/m-K

@Temperature 482 °C
157 BTU-in/hr-ft²-°F

@Temperature 900 °F
condition H 900
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1025 (Heated 552°C)
Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio..