Polymer Property : Thermal Conductivity = 14.6 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 14.6 W/m-K

@Temperature 300 °C
101 BTU-in/hr-ft²-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked
Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 14.6 W/m-K

@Temperature 300 °C
101 BTU-in/hr-ft²-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked
Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 14.6 W/m-K

@Temperature 300 °C
101 BTU-in/hr-ft²-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked
Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 14.6 W/m-K

@Temperature 300 °C
101 BTU-in/hr-ft²-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked
Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Thermal Conductivity 14.6 W/m-K

@Temperature 300 °C
101 BTU-in/hr-ft²-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.