Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 131.7 W/m-K @Temperature 300 °C |
914.0 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
Thermal Conductivity | 131.7 W/m-K @Temperature 300 °C |
914.0 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |