Thermal Properties Metric English Comments
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 1.6 mm sheet
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 12.7 mm (1/2 in.) thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 12.7-50.8 mm bar
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 19.1 mm thick plate, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, 6.3-38.1 mm plate
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 204°C (400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 316°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 427°C (800°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 538°C (1000°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 649°C (1200°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 760°C (1400°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 871°C (1600°F)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, aged 1000 hours at 982°C
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, all-weld metal, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, all-weld metal, GTAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, all-weld metal, SMAW weld
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, mill annealed
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, plate, GMAW weld (short)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Ultimet® alloy, plate, GMAW weld (spray)
Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio..
Thermal Conductivity 13.8 W/m-K

@Temperature 20.0 - 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Thermal Conductivity 13.8 W/m-K

@Temperature 20.0 - 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310H Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Thermal Conductivity 13.8 W/m-K

@Temperature 20.0 - 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Thermal Conductivity 13.8 W/m-K

@Temperature 20.0 - 100 °C
95.8 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..