Thermal Properties Metric English Comments
Thermal Conductivity 1.83 W/m-K

@Temperature 1093 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable
Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol..
Thermal Conductivity 1.83 W/m-K

@Temperature 650 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 60 A Dense Refractory Brick
Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% ..
Thermal Conductivity 1.83 W/m-K

@Temperature 1100 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 60 A Dense Refractory Brick
Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% ..
Thermal Conductivity 1.83 W/m-K

@Temperature 650 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Gouda Vuurvast AK 60 AP Dense Refractory Brick
Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime ..
Thermal Conductivity 1.83 W/m-K

@Temperature 1100 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Gouda Vuurvast AK 60 AP Dense Refractory Brick
Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime ..
Thermal Conductivity 1.83 W/m-K

@Temperature 1093 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable
Pyrocast AL2 refractory castable is a mullite-based refractory well suited for applications prone to erosion and abrasion. It exhibits excellent non-wetting properties when used in molten aluminum ..
Thermal Conductivity 1.83 W/m-K

@Temperature 1093 °C
12.7 BTU-in/hr-ft²-°F

@Temperature 1999 °F
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable
Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low..