Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.83 W/m-K @Temperature 1093 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 1999 °F |
|
Pyrotek Pyrocast ALF2 Low Cement Refractory Castable Pyrocast ALF2 is a low cement castable with mullite base. It is suited for applications requiring high strength at elevated temperatures and abrasion resistance.ApplicationsAluminum melting and hol.. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 650 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% .. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 1100 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% .. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 650 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 1200 °F |
|
Gouda Vuurvast AK 60 AP Dense Refractory Brick Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime .. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 1100 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Gouda Vuurvast AK 60 AP Dense Refractory Brick Description: This phosphate bonded brick combines a very good thermal shock resistance with high slag resistance and low creep. Application: frit melting furnaces, incinerators, burner blocks, lime .. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 1093 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 1999 °F |
|
Pyrotek Pyrocast AL2 Abrasion-Resistant Refractory Castable Pyrocast AL2 refractory castable is a mullite-based refractory well suited for applications prone to erosion and abrasion. It exhibits excellent non-wetting properties when used in molten aluminum .. |
|||
Thermal Conductivity | 1.83 W/m-K @Temperature 1093 °C |
12.7 BTU-in/hr-ft²-°F @Temperature 1999 °F |
|
Pyrotek Pyrocast AL3 Abrasion & Alkali Resistant Refractory Castable Pyrocast AL3 is suited for use in aluminum melting equipment and metal transfer areas where sever wear or alkali attack are a factor. Pyrocast AL3 is a high-purity mullite based refractory with low.. |