Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.40 - 1.60 W/m-K @Temperature 600 °C |
9.72 - 11.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS PBK D Moldable Refractory Material Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. This moldable contains a phosphate binding agent and has a low silica cont.. |
|||
Thermal Conductivity | 1.40 - 1.60 W/m-K @Temperature 600 °C |
9.72 - 11.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS PBK DGM Moldable Refractory Material Description: This material is supplied as a dry gunning powder. This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in goo.. |
|||
Thermal Conductivity | 1.40 - 1.60 W/m-K @Temperature 1200 °C |
9.72 - 11.1 BTU-in/hr-ft²-°F @Temperature 2190 °F |
|
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values .. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 Dense Vibrating Refractory Castable Description: Vibron 160 is a low cement vibrating castable on andalusite base, characterized by a high strength and excellent thermal shock resistance.Remarks: Indicated values apply to vibrated pro.. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 H Dense Vibrating Refractory Castable Description: Vibron 160 H is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance.Remarks: Indicated values apply to vib.. |
|||
Thermal Conductivity | 1.40 - 1.60 W/m-K @Temperature 600 °C |
9.72 - 11.1 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast CURAS PBK Moldable Refractory Material Description: This moldable contains a phosphate binding agent and has a low silica content. For a large variety of applications this results in a good slag resistance and high strength properties at.. |
|||
Thermal Conductivity | 1.50 - 1.60 W/m-K @Temperature 1400 °C |
10.4 - 11.1 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Gouda Vuurvast VIBRON 160 H RAPID Dense Vibrating Refractory Castable Description: Vibron 160 H Rap is a low cement castable based on high fired high alumina grog and characterized by a high strength and good thermal shock resistance. Because of special additives, thi.. |