Thermal Properties Metric English Comments
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-105C PET Bottle Grade
A co-polymer used for soft drinks and other applications.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-109JS PET Sheet Grade
Used mainly for 5 to 20 liter mineral water containers
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-113C PET Sheet Grade
Used mainly for box strapping.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET D-101-SH Monofilament Resin
Used in the paper industry as paper pulp nets.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET F097H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET F097HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET FR-101-H Monofilament Resin
Used as textile grade flame retardant for furniture, car and plane upholstery.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-101C PET Sheet Grade
A sheet grade polymer used in thick films.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B101H Monofilament Resin
Generally used in monofilament v-belts, zips and other technical applications.
Thermal Conductivity 0.213 W/m-K

@Temperature 280 °C
1.48 BTU-in/hr-ft²-°F

@Temperature 536 °F
liquid
Pearl Engineering PEPLPET B-103C PET Bottle Grade
A co-polymer used for mineral water bottles