Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.18 - 1.38 W/m-K @Temperature 600 °C |
8.19 - 9.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis.. |
|||
Thermal Conductivity | 1.18 - 1.38 W/m-K @Temperature 600 °C |
8.19 - 9.58 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast FLUCON 160 H Dense Self Flowing Refractory Castable Description: Flucon 160 H is a self-flowing low cement castable on high fired high alumina grog base, characterized by a high strength and good thermal shock resistance.Remarks: These values apply t.. |