Polymer Property : Thermal Conductivity = 1.04 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.150 W/m-K

@Temperature 980 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Pyrotek PTB 2200 Structural Board
ApplicationsCaster tips Small machined nozzles Slotted caster tips AdvantagesHigh strength Resistant to thermal shock Easily machined Non-wetting to molten non-ferrous metals Low thermal mass High t..
Thermal Conductivity 0.150 W/m-K

@Temperature 650 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1200 °F
Mid-Mountain Materials CERMEX® PR1000-P Premium Grade Thermal Insulation Paper
Material: Non-respirable E-glass fibers Construction: Felted paper, organic binderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.150 W/m-K

@Temperature 400 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group Moler BF-BLOCK Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.150 W/m-K

@Temperature 400 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group V-1100 410 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.150 W/m-K

@Temperature 400 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-201 supplemented by ASTM C-182
Skamol Group VERMICAST 116-25 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Thermal Conductivity 0.150 W/m-K

@Temperature 400 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
Skamol Group Moler SM-65 Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Thermal Ceramics Ceraboard P
Ceraboard P has tighter thickness tolerances and s particularly useful in applications requiring very low variability. It is made from a slurry of refractory fibers and binders which have a low orga..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Thermal Ceramics Kaowool 1401 Millboard
Kaowool 1401 Millboard is a strong, thin, dense board product with excellent compression resistance and insulating characteristics. It is produced from Kaowool ceramic fibers, clay, inert fillers, a..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc R
Pyro-Bloc Veneering modules, R Grade, ZR Grade, C Grade are made Pyro-Log fiber turned edge-grain and slightly compressed with a gauze type wrap. Pyro-Bloc Veneering Modules are part of the Unisyste..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc R M and M2 Modules
The Pyro-Bloc M and M2 modules are a ceramic fiber lining system designed for high-temperature furnaces that require corrosion barriers on the shell. The module is manufactured from a high-purity bl..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc R T-Bar Module
Features:Monolithic, edge-grained ceramic fiber module Available in uncompressed densities from 8 to 15 pcf (128 - 240 kg/m3)Easy access attachment allows quick installation over coated shells Insta..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc R Y and Y2 Modules
The Pyro-Bloc Y and Y2 modules are manufactured from a high purity blend of raw materials which are used to produce R Grade (alumina-silica) ceramic fibers. The modules utilize a specially designed ..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc ZR
Pyro-Bloc Veneering modules, R Grade, ZR Grade, C Grade are made Pyro-Log fiber turned edge-grain and slightly compressed with a gauze type wrap. Pyro-Bloc Veneering Modules are part of the Unisyste..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Bloc ZR Y and Y2 Modules
The Pyro-Bloc Y and Y2 modules are manufactured from a high purity blend of raw materials which are used to produce ZR Grade (alumina-zirconia-silica) ceramic fibers. The modules utilize a specially..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Log R Fiber
Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm to 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3). Manufactured in three t..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Log ZR Fiber
Pyro-Log is an uncompressed monolithic mass of ceramic fiber. Pyro-Log fiber is available in 6" and 8" (152 mm to 203 mm) thicknesses with densities up to 15 pcf (240 kg/m3). Manufactured in three t..
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
10 pcf; ASTM C201
Thermal Ceramics Pyro-Packing R
Pyro-Packing is used to fill gaps or small spaces in ceramic fiber module linings where standard shapes are not practical or cost effective. Manufactured by cutting pieces of monolithic Pyro-Log, Py..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C201
Thermal Ceramics Superwool 607 Board
Superwool boards are processed from a slurry consisting of Superwool bulk and organic binders. Each board has cut edges for controlled squareness and trueness. Boards up to 36” wide may be ordered ..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C201
Thermal Ceramics Superwool 607 Flex-Wrap Paper
Superwool Papers are uniquely designed from Superwool bulk and organic binders in a unique paper making process. Superwool Papers are specially processed to offer excellent performance in high-tempe..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C201
Thermal Ceramics Superwool 607 Paper
Superwool Papers are uniquely designed from Superwool bulk and organic binders in a unique paper making process. Superwool Papers are specially processed to offer excellent performance in high-tempe..
Thermal Conductivity 0.150 W/m-K

@Temperature 816 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C201
Thermal Ceramics Superwool 612 Board
Superwool boards are processed from a slurry consisting of Superwool bulk and organic binders. Each board has cut edges for controlled squareness and trueness. Boards up to 36” wide may be ordered ..
Thermal Conductivity 0.150 W/m-K

@Temperature 856 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1570 °F
Thermal Ceramics TR-20 Block Insulation
TR-20 Block is a superior, high-temperature insulation for service to 2000°F (1095°C). According to ASTM testing procedures, TR-20 exhibits extremely high resistance to breakage to 2000°F (1095°..
Thermal Conductivity 0.150 W/m-K

@Temperature 200 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials BNZP-23L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.150 W/m-K

@Temperature 427 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 801 °F
BNZ Materials Marinite® C Ceramic Board for Aluminum Contact
These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuou..
Thermal Conductivity 0.150 W/m-K

@Temperature 600 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1110 °F
3M Nextel™ BF-30 Woven Fabric 440
Information provided by 3M
Thermal Conductivity 0.150 W/m-K

@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F

@Temperature 1000 °F
6 pcf
Thermal Ceramics Kaowool Blanket
Kaowool blanket is produced from kaolin, a naturally occurring alumina-silica fire clay. Kaowool, the world’s most recognizable name in ceramic fiber blanket, is available in a wide variety of dens..