Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.02 W/m-K @Temperature 100 °C |
7.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast B Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1300°C.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda.. |
|||
Thermal Conductivity | 1.02 W/m-K @Temperature 300 °C |
7.07 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Stellar Canada CERAMITE® SFR Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |