Polymer Property : Thermal Conductivity = 0.710 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.710 W/m-K

@Temperature 550 °C
4.93 BTU-in/hr-ft²-°F

@Temperature 1020 °F
Pyrotek Pyrocast AR Castable Refractory
Pyrocast AR is a fused silica castable refractory inert to liquid aluminum and its alloys. It is a high strength material offering resistance to erosion and mechanical damage. Parts cast from Pyro..
Thermal Conductivity 0.710 W/m-K

@Temperature 550 °C
4.93 BTU-in/hr-ft²-°F

@Temperature 1020 °F
Pyrotek Pyrocast AR FINE Castable Refractory
Pyrocast AR Fine is a fine-grain fused silica castable, offering similar insulation properties, yet lighter weight that the Pyrocast AR formulation. Pyrocast AR Fine is suited for thin wall casting..
Thermal Conductivity 0.710 W/m-K

@Temperature 1038 °C
4.93 BTU-in/hr-ft²-°F

@Temperature 1900 °F
Zircar Ceramics ZIRALCAST 95 Alumina Refractory Castable
Hydraulically setting castable refractory containing high purity fused alumina "bubbles". This low density castable can be used like concrete and produces ceramic bodies useful in a range of applica..