Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.690 W/m-K @Temperature 540 °C |
4.79 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrocast ICL Castable Refractory Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist.. |