Thermal Properties Metric English Comments
Thermal Conductivity 0.620 W/m-K

@Temperature 295 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 563 °F
Pyrotek Pyrocast ICL Castable Refractory
Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resist..
Thermal Conductivity 0.620 - 0.720 W/m-K

@Temperature 1300 °C
4.30 - 5.00 BTU-in/hr-ft²-°F

@Temperature 2370 °F
Gouda Vuurvast CURON 140 GM Dense Refractory Castable
Description: Because of its relatively low Fe2O3 content and its high alumina percentages, this gunning castable can be applied up to 1400°C in slightly reducing atmospheres.Remarks: These values..
Thermal Conductivity 0.620 W/m-K

@Temperature 200 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 392 °F
parallel to thickness
Zircar Refractory Composites RS-1200 Refractory Sheet
ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12..
Thermal Conductivity 0.620 W/m-K

@Temperature 1093 °C
4.30 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-32 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..