Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.476 W/m-K @Temperature 1600 °C |
3.30 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Zircar Zirconia Buster Blanket Alumina Blanket Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |
|||
Thermal Conductivity | 0.476 W/m-K @Temperature 1600 °C |
3.30 BTU-in/hr-ft²-°F @Temperature 2910 °F |
|
Zircar Zirconia Buster Blanket Alumina Blanket Insulation Buster Blanket and Buster Mat are flexible, Hi-Alpha alumina fiber insulation materials. The mat is 100% fibers while the blanket has been needled into a durable blanket with the addition of an orga.. |